we required repairs on a 48-inch diameter stub-in weldment and the last repair passed the ndt. however, the system was put on line after the repairs passed the ndt so we can minimize generation losses.
what will be the effect of not stress relieving the joint with four repairs? will a leak or crack eventually occur? the design temperature is 214MPag (310psig) and 216degC (420degF).
thanks.