I do not know how to calculate the thitening torque of the foundation anchor bolt (J shape)in concrete type 250 Rck. Best regard fhfag20
Jul 14, 2003 #2 jrmack Structural Joined Jun 10, 2001 Messages 32 Location CA For anchor bolts, snug tight should be enough. With concree shrinkage and creep, a bolt tension corresponding to a specified torque would be lost over time. Upvote 0 Downvote