Foundation anchor bolts

Status
Not open for further replies.

fhfag20

Structural
Joined
Feb 13, 2003
Messages
6
Location
IT
I do not know how to calculate the thitening torque of the foundation anchor bolt (J shape)in concrete type 250 Rck.
Best regard
fhfag20
 
For anchor bolts, snug tight should be enough. With concree shrinkage and creep, a bolt tension corresponding to a specified torque would be lost over time.
 