ElCidCampeador
Mechanical
Hi, I'm trying to find out the forming strain according to equations of table UG-79-1, ASME VIII div.1 Ed.'15.
Case: hemispherical head formed from pipe (A 333 Gr.6).
What are Rf and R0? I mean, Rf=R final sphere, but R0? At the beginning I have a pipe, not a plate, so it's not equal to infinite, isn't it? Thank you
Case: hemispherical head formed from pipe (A 333 Gr.6).
What are Rf and R0? I mean, Rf=R final sphere, but R0? At the beginning I have a pipe, not a plate, so it's not equal to infinite, isn't it? Thank you