1
- #1
KevinHowick
Industrial
customer would like to form 0.2mm thick 301 s.s. and acheive spring properties using full hard material. I do not think this will work without the material cracking at the tight bends that are required. I have both good way and bad way bends
Thought was to use a 17/7 PH annealed grade and then heat treat after forming to obtain the sring properties to the part withour distortion through heat treat.
Any other options of material I should consider?
Thanks.
Thought was to use a 17/7 PH annealed grade and then heat treat after forming to obtain the sring properties to the part withour distortion through heat treat.
Any other options of material I should consider?
Thanks.