Is it possible to hang slab soffit formwork from steel beams? It seems to me that 40 years ago this was routinely done with inverted U hangers over the top of the steel beams, but today contractors don't seem to want to do it. We don't want to use steel deck as a form because we are putting a urethane waterproofing membrane on the top side of the new concrete slab, and the soffit therefore must be left free to breathe (as per CSA Standard S413). The new slab is 5 storeys up, so forming it from the ground level below would not seem economical.