Hello,
We do a lot of work for this manufacturer. They have in house engineers but they aren't PE's in some states, which is where our firm comes in. We will stamp drawings/calcs for states they aren't PE's in.
Problem: They are taking 3/8" and 5/16" plate and bending them into channels. They word it like this "(C10) Designation represents a SS 3/8" formed plate to match C10x15.3 Channel."
The steel is SS type 304L.
Two questions:
1) Does this constitute a cold formed section now? Should I design with AISI?
2) More importantly, does this type of steel even allow cold forming? Are you allowed to form sections this thick? It seems to me you will get significant yielding at the outside corners since the sections are much much thicker than cold formed sections. Aren't there ductility requirements for cold formed sections? Are my concerns valid?
They've maybe done this once before or twice before but for some reason I didn't take issue with it. I'm going to talk to my boss about it in a bit but I was also like to hear what the community has to say about this.
Thanks in advance!
We do a lot of work for this manufacturer. They have in house engineers but they aren't PE's in some states, which is where our firm comes in. We will stamp drawings/calcs for states they aren't PE's in.
Problem: They are taking 3/8" and 5/16" plate and bending them into channels. They word it like this "(C10) Designation represents a SS 3/8" formed plate to match C10x15.3 Channel."
The steel is SS type 304L.
Two questions:
1) Does this constitute a cold formed section now? Should I design with AISI?
2) More importantly, does this type of steel even allow cold forming? Are you allowed to form sections this thick? It seems to me you will get significant yielding at the outside corners since the sections are much much thicker than cold formed sections. Aren't there ductility requirements for cold formed sections? Are my concerns valid?
They've maybe done this once before or twice before but for some reason I didn't take issue with it. I'm going to talk to my boss about it in a bit but I was also like to hear what the community has to say about this.
Thanks in advance!