Apr 14, 2021 #1 U2tree Industrial Joined Mar 4, 2011 Messages 13 Location US this is 11 ga pickled and oiled sheet anyone ever see this happen or know what might cause it??
Apr 14, 2021 #2 mfgenggear Aerospace Joined Jan 23, 2008 Messages 3,607 Location US yes I use to Inspect sheets and Plates for delamination from the mill. it was common, pull the raw stock and have it visual inspected. Upvote 0 Downvote
yes I use to Inspect sheets and Plates for delamination from the mill. it was common, pull the raw stock and have it visual inspected.
Apr 22, 2021 #3 gtaw Structural Joined Feb 10, 2006 Messages 1,988 Location US A quick thickness test using a ultrasonic thickness mic using a dual element transducer can detect laminations in many thickness ranges, but probably not the best choice for materials least than 1/8-inch thick. Best regards - Al Upvote 0 Downvote
A quick thickness test using a ultrasonic thickness mic using a dual element transducer can detect laminations in many thickness ranges, but probably not the best choice for materials least than 1/8-inch thick. Best regards - Al