First time I am posting here. Any help on the following problem will be much appreciated.
I am trying to simulate forming (actually crimping) anlysis on an assembly of components. Its 2D analysis with and during analysis is exiting stating time increment required is smaller than specified (specified min -1e-05). Also it is showing elements sticking between punch and component (right now I have given penulty friction of 0.05). Should I increase the friction or change meshing or do something else. (I am using relatively fine meshing in that area).
Thanks again
Dipak
I am trying to simulate forming (actually crimping) anlysis on an assembly of components. Its 2D analysis with and during analysis is exiting stating time increment required is smaller than specified (specified min -1e-05). Also it is showing elements sticking between punch and component (right now I have given penulty friction of 0.05). Should I increase the friction or change meshing or do something else. (I am using relatively fine meshing in that area).
Thanks again
Dipak