Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Formigli Longspan channel crete

Status
Not open for further replies.

l21615

Structural
Mar 23, 2009
1
Has anyone ever heard of this? I have this one span table. I'm also looking for information on precast tongue and groove concrete plank. Would they have put any mesh in there or would it be plain concrete?
 
Replies continue below

Recommended for you

never heard of it.

that span table looks like it was published in the 70's.
 
It looks like precast roof panels, I saw it once during a roof remodelling project for a water treatment plant. It stayed well, but the foam insulation and water proofing were deteriorated. vandede427 are correct, it was produced around 70's.
 
It may be a residential system, many attempts have been made to come up with lightweight flooring systems. Try ACI?. Would be interested to see what turns up.
 
Curiousity got to me. Google led to a acquistion of Formigli by the High Group. You
might try contacting them, they supposedly acquired Formigli in 1982.
 