Sep 20, 2021 #1 Ed555 Industrial Joined Sep 20, 2021 Messages 9 Location US Good afternoon, How is 'material worked sufficiently to remove the coarse ingot structure' defined? Is it verified by determining the grain size of the material? Also, does a material used for an ASME B16.5 flange meet this requirement? Thank you,
Good afternoon, How is 'material worked sufficiently to remove the coarse ingot structure' defined? Is it verified by determining the grain size of the material? Also, does a material used for an ASME B16.5 flange meet this requirement? Thank you,
Sep 21, 2021 #2 Dhurjati Sen Materials Joined Dec 14, 2017 Messages 1,005 Location IN 1. Google 'forged flanges'. 2. Yes. DHURJATI SEN Upvote 0 Downvote