I don't have a lot of experience with the forging process. I learned about it way back in school, but professionally, I have not been involved with forgings too much, so this might sound like a dumb question. Can you create a forging using two pieces of dissimilar metals? Sort of like an insert mold. I am looking at a specialized hub for a wheel chair wheel. The current piece is an aluminum forging. I would like to put a steel insert into the part. Is this even possible?
Thanks.
rShell
Thanks.