Spainers87
Civil/Environmental
Hi All,
We need to test a newly installed water distribution main. It is cement lined ductile iron (500mm). There are some issues with the mortar lining coming away from the pipe. The pipe hasn't been commissioned yet but we expect flows of 400-500l/s.
We are worred about further deterioration and damage to the large PRV downstream.
We need to test a seciton of the pipe to see the effect on the mortar of design flows. We can get flows of 100 l/s for testing so would need to create a blockage of approx 80% to have a flow velocity broadly equivalent to 500 l/s.
Unsure yet how to create the blockage but to do that I would like to estimate the force experienced by the blockage under the flows indicated.
Any ideas? Thank you in advance.
We need to test a newly installed water distribution main. It is cement lined ductile iron (500mm). There are some issues with the mortar lining coming away from the pipe. The pipe hasn't been commissioned yet but we expect flows of 400-500l/s.
We are worred about further deterioration and damage to the large PRV downstream.
We need to test a seciton of the pipe to see the effect on the mortar of design flows. We can get flows of 100 l/s for testing so would need to create a blockage of approx 80% to have a flow velocity broadly equivalent to 500 l/s.
Unsure yet how to create the blockage but to do that I would like to estimate the force experienced by the blockage under the flows indicated.
Any ideas? Thank you in advance.