Hi,

I have some 0.2mm (0.008 inch) thick stainless steel that I want pressed or stamped flat. It is flatish now but I want it 100% flat. The parts are just 3cm / 1 inch diameter and I don't want to send them out to be done. I want to buy a cheapish fly press or stamping machine. What would you recommend? I mean how much press do I need to get 0.2mm stainless 100% flat? I don't want to spend more than £200, $300 unless I have to. And how much is the thickness going to change?

Regards,

Ant.
 
Agree. Thanks for the spot on comments. Regards, Ant.
 
If you really want them flat then lapp them. adding force will change the distortion but not likely get them any flatter.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
If you're serious about your flatness range then I'm not sure pressing will do it. If you really need to get down I think you probably need to grind or even lap as Ed says.

Posting guidelines faq731-376 (probably not aimed specifically at you)
What is Engineering anyway: faq1088-1484
 
Flatness can be measured by the difference in height from edge to edge or to center line.


Look into "coining" - the US Mint does a pretty good job of this....
 
If they had been fine blanked in the first place they would be flat.
I would still try to lap them, you will get flatness better than you can measure and there is no tooling, just machining costs. Very low stress process also.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
If a 12" square of 0.020" shim stock is not flat, it will not be made flat by lapping. Just one example.
 
These are 1" diameter, easy enough to polish flat by hand.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Since you indicated an intention to coin the parts at a later process step, I fail to see the added value of lapping or even pressing them 'flatter' now.



Mike Halloran