Anyone familiar with this material. It has been quoted as a superior replacement for manganese bronze and super oilite #16 in the following application.
Rotating castor
1500 RPM
400 psi
Drilling mud with solids (barite)
Max temp 350F
PV = 628,000
7100 is a very hard plastic from what I'm told. It has a compressive strength of 43,000. I just can't see plastic lasting very long.
Note: A multi-layer 04DU04 Steel backed sintered bronze and PTFE bearing was worn away in 3 hours in this environment. In same application but in oil (produced crude) the 04DU04 works fine.
Thoughts???