Am testing for leaks using fluorescent dye penetrant (spray can application) on exterior of 3/16" thk. 304L matl 10' dia x 18' L vessel and using black light to reveal discontinuities from interior.
In the past the Magnaflux Zyglo penetrant would reveal even minor, minute cracks within 4 hrs.
I checked the vessel skin and it reads 48-50 deg F.
Tried warming up suspected areas (T-joints intersections) to approx 80 deg F and performed PT, same results, does not reveal discontinuities till dwell times of 2-5 days!
Appreciate any advice or suggestions from those with experience using fluorescent dye penetrant....
Have changed batch number for PT and still same results.
Would using the white developer work with fluorescent dye penentrant? If so, would it reveal cracks faster?
Have Paint Dept wanting vessel for glass bead blasting but cannot release it till I am assured of integrity.
In the past the Magnaflux Zyglo penetrant would reveal even minor, minute cracks within 4 hrs.
I checked the vessel skin and it reads 48-50 deg F.
Tried warming up suspected areas (T-joints intersections) to approx 80 deg F and performed PT, same results, does not reveal discontinuities till dwell times of 2-5 days!
Appreciate any advice or suggestions from those with experience using fluorescent dye penetrant....
Have changed batch number for PT and still same results.
Would using the white developer work with fluorescent dye penentrant? If so, would it reveal cracks faster?
Have Paint Dept wanting vessel for glass bead blasting but cannot release it till I am assured of integrity.