Pressure Calcs for Formwork for Flowable Fill

Flowable Fill, 150 psi, weight 110 pcf, slump 9"

Formwork Max Pressure = Cc X Cw x (150 + 9000 x R / T)

What T to use?
Even though this is the fill material temp, would it be likely to be close to air temp because cement content is low? So 50 deg, NYC, now.

Cw = 0.5 x (1+ 110/145) = 0.88
Cw = 1.4 (additives in mix)

What R?
Or should I just use liquid analogy, P = 1/2 weight x height^2, and not bother with the above?

I need to be conservative on this. Any form bust is very serious in this location.

Total Height 10 ft, planning on (2) 5 ft high pours 24 hrs apart, Is this enough time for curing?

 
Replies continue below

Recommended for you

With flowable fill you will not realize much benefit from adjusting "R". Because of the low cement content, it will not set up fast enough for R to be useful. Because of this, either use a fast R or just take the full liquid approach.

 
Thanks, especially for ACI document to review.
Fast R and liquid approach pretty much get the same force. And using T as close to ambient air temp is conservative even if technically not correct.
Curing time? 24 hrs? 48 hrs? Anybody know.
 
Ron, yup... even if I'd consider this as SCC... full hydrostatic load without the max 'cut-off'.

image_m2lutb.png


Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?

-Dik
 
24 hours for flow fill usually enough but those are for mud slab of foundation.
 
Thanks,
This going into a sidewalk vault to be abandoned, under a New York City street.
 