I currently have an issue where an H2SO4 - 98% >70 deg C line has eroded at elbows/welds etc from flow induced erosion due to the velocity and volume of acid travelling through the pipe. I am looking to replae this line though currently have conflicting advice on maximum allowable flows prior to the onset of internal flow induced erosion. The max ranges I have been given for carbon steel are 0.6 - 1.0m/s and for 316L are 1.0-2.0m/s. Anybody have any experience with this.
Regards and many thanks
JonD
JonD 71
Australia
Regards and many thanks
JonD
JonD 71
Australia