I AM LOOKING FOR A COST EFECTIVE COATING FOR A SECONDARY CONTAINMENT
AREA : STORAGE AREA WITH BURMS TO BE COATED.CHEM: NITRIC ACID 60% ...
TO BE STORED IN DRUMS IN THIS AREA.
 
I respectfully suggest you contact a company we here at BP use, they deliver worldwide for this application.
Company Name: Chemco International
Telephone No. + 44 (0)1236 606060
Facsimile No. + 44 (0)1236 606070
E-mail. chemcoint@aol.com
Contact Name: Manny Khorasani.

I am a specifying engineer, and have found these people to be very helpful in the past, especially with difficult to treat areas.
Regards,
Rembrandt.
 
THANK YOU REMBRANDT, I WILL GIVE THEM A CALL
GREGNAGOR
 
I am new to the forum method and hope that this is helpful. I have worked as a coating formulator for over 30 years and have designed many coatings for containment areas. check sales@blome.com This is Blome International and they are first class in floor coatings for severe exposure conditions.
 
I have a lot of experience with hi resin containing coatings like "Overkote". these coatings are self leveling and will hold up to a lot of abuse.
Coating thickness and resin content are what will get you a good result. If you want more information please contact me at sheger@hegerpumps.com