Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Flitch Plate/Beam Design 1

Status
Not open for further replies.

pruho

Structural
Jun 8, 1999
3
I have designed flitch beams for residential construction for 10 years, but have not located any useful references specifically related to this subject matter. Should anyone know of good design literature on this subject, such information would be greatly appreciated. Thanks. John
 
Replies continue below

Recommended for you

"Flitch Plate and Steel I-Beams" is a manual by National Association of Home Builders, 15th and m Streets, NW, Washington D.C. 20005. Also, article in Civil Engineering magazine, September 1989.
 
Also check out:
"Wood Engineering and Construction Handbook" by Faherty & Williamson
and
Timber Design and Construction Handbook bt Timber Engeneering Company.

Both are available on "out of print" search engines.
Both are published by McGraw-Hill and are very good references. [sig][/sig]
 
I do not design a lot of flitch beams but recently designed one using Superbeam 4 software and a hand check of the results.
A building control officer, who will remain nameless, is insisting that "in his experience" the plate I have used is not thick enough but he refuses to back this up with any calculation.
Did you find any good literature following your previous query? If so I could do with a copy to appease aforementioned annoying b.c. officer!
 