quiteone
Industrial
- Jun 6, 2005
- 3
A number associated with the flexibilty or stiffness of a material.The lower the number the more flexible, the higher the less flexible, my question is
Dose this number affect the shrinkage of plastic materials,
I.E the higher the number the more shrinkage you get??
Have just sampled two new plastic resins with the FM# higher than the regular resin that i use and both have shown more shrinkage, than the regular resin.
Any thoughts on this. All 3 materials share the same MFI and density etc the only differance is the FM# regular material is 1150 new materials are 1400 and 1450.
Dose this number affect the shrinkage of plastic materials,
I.E the higher the number the more shrinkage you get??
Have just sampled two new plastic resins with the FM# higher than the regular resin that i use and both have shown more shrinkage, than the regular resin.
Any thoughts on this. All 3 materials share the same MFI and density etc the only differance is the FM# regular material is 1150 new materials are 1400 and 1450.