Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

flexture strength 1

Status
Not open for further replies.

hanaria

Mechanical
Joined
Apr 30, 2001
Messages
5
Location
ID
Dear sirs,
I'd like to know about flexture strength. What is the flexture strength? How to test it? How to use it? Is it related to modulus of something? Thanks
 
Flexure "strength" as you put it, is, in a nutshell, how much stress a beam or similarly-acting structural member can take before it breaks. ASTM D790 is a good place to start.
 
There are many ASTM standards associated with flexural strength, so it depends upon the material you are testing. The one noted by DaveViking (D790) is related to the flexural strength of plastics and insulating materials. Since you asked about a specific modulus, I will answer your question with the assumption that you are testing concrete, since the flexural strength of concrete and its modulus of rupture are commonly interchanged terms.

The test for flexural strength most commonly used for concrete is ASTM C78, the "third-point" loading test. From this test, you can determine the modulus of rupture of the concrete in flexure. This is a commonly specified parameter for rigid pavement design. Typically, the modulus of rupture should exceed about 500 psi for standard duty rigid pavements, and should be greater than 650 psi for airfield or industrial pavements.

There are other similar standards in ASTM for concrete, particularly ASTM C293 for center point loading, and ASTM C1018 for flexural toughness and first crack index of fiber reinforced concrete.
 