Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Flexible 3.3 KV, 95 sq mm rubber insulated copper cables 3

Status
Not open for further replies.

edison123

Electrical
Oct 23, 2002
4,508
Can anyone suggest websites for flexible 3.3 KV rubber insulated copper cables for 95 sq mm and above ? Any personal experiences with these cables will be appreciated.
 
Replies continue below

Recommended for you

Take a look at Pirelli cables, should be easy to find on the internet.

They have single and 3 phase with and without F.O.

kind regards,

Danny
 
Edison123

Trailing/Reeling cables?

We use trailing cables on our showels and drills (Mining, 3.3kV and 6.6kV)

I do not know where you are located, but if you are in Southern Africa, you can contact Aberdare cables. We use a rubber cable (type 66) for our 6.6kV shovels. (their site is but I haven't seen this cable info on their site, you have to contact them)

You can also visit: ( search for rubber cables)
Cable name: Tenax

You'll find info under:
(N)TS…WOEU
NTS…WOEU
(Open left-side colomn)

Regards
Ralph
 
Thx Danny & Ralph.

I should have mentioned single core cables. sorry.

Kumar
 
Kumar

At the Drakakabely-site, see the last product:
NTMCWOEU***
However, it is rated for 10 or 20kV

I'm sure you'll find also useful info at okonite (
What do you want to do with the cable?

Regards
Ralph
 
Thx Ralph. I want to use this cable for loop tests on large generators where I expect to have volatges around 2 KV max. So, I need lots of flexibility to wind around the cable stator core. At Drakakabely site, all the links go back to the same page (list of items). Okonite sounds interesting. Will get back after I talk to them. Thx once again.



 
Kumar

Just click once on the lefthand colomn. I've noticed that if you open it in a new page, it goes back to the main page.

How long is the piece you want to use? If it is not that long, and if you have 3-core cable on site, (size you want to use and bigger than 3kV) strip the cable and use the tails. Just remember to strip semi-conductor jacket also and to clean it.

Regards
Ralph
 
 
There is a robust semi-flexible 2kV-rated unshielded cable termed “DLO” {diesel locomotive cable} sized from 14AWG (~2mm²) to 1111kcmil (~550mm²). This “2-pass” cable with Individual stranding of 24AWG with EPR-dielectric/CSPE-jacket that is very likely available in mm² sizes.

Example
 
Thx Ralph. The site still doesn't work. May be my computer problem. Problem using the 3 core is the termination.


busbar

Thx for a very good reference. It was exactly I was looking for.
 
busbar

I am finalzing order on elektrimna on DLO 95 sq mm single core cable. Thx once again for a good reference.

Danny & Ralph

Thx you too for your good references. I have bookmarked them for future use.

Kumar
 