Hi All,
We are in process of producing a heat treated flat bar made from Cast Iron(FG260).
This cast iron bar is used for supporting the conveyor belt in an Industrial oven.
The cast iron bar is machined as per the drawing & heat treated by Induction hardening to 1.5 mm case depth.
The length of the cast iron bar is 1200mm, width of the bar is around 70mm.
After the heat treatment, the flatness measured is up to 3mm along the length of the cast iron bar.
Can anyone advice Flatness tolerance after heat treatment(Induction hardening)?
We are unable to decide whether to accept or reject the part.
Thank you
We are in process of producing a heat treated flat bar made from Cast Iron(FG260).
This cast iron bar is used for supporting the conveyor belt in an Industrial oven.
The cast iron bar is machined as per the drawing & heat treated by Induction hardening to 1.5 mm case depth.
The length of the cast iron bar is 1200mm, width of the bar is around 70mm.
After the heat treatment, the flatness measured is up to 3mm along the length of the cast iron bar.
Can anyone advice Flatness tolerance after heat treatment(Induction hardening)?
We are unable to decide whether to accept or reject the part.
Thank you