Gooday everyone.
I have a real "blast from the past" here.
Can anyone help me with the head heights for AN442-3,-4,-5 and -6 rivets. This is an old defunct standard that I cannot lay my hands on.
I am trying to arrive at some damage limits for universal head rivets which have been sanded.
Thanks all.
 
Replies continue below

Recommended for you

Gooday Graeme,

Old is right! This spec was cancelled in 1959!

For 3/32, head height is .038" +/-.005
For 4/32, .050" +/-.005
For 5/32, .062" +/-.005
For 6/32, .075" +/-.005

Hope that helps.

SuperStress
 
Thanks Superstress.
That fitted the bill perfectly
 