I have a diaphragm disk, .0625" thick, 4.944" diameter, 17-4 PH H-900. I fixed the very edge around the diameter, the .0625" thick OD edge, and put 50 psi on one face. I end up with .004" max deflection in the very center. That seemed low so I had a friend run the same test on Pro-E and he came up with .042" which seems correct. Hmmm, off by a factor of 10???
I check units, pressure, etc. and everything seems OK.
Could someone run this piece and see what they get?
Thanks!
I check units, pressure, etc. and everything seems OK.
Could someone run this piece and see what they get?