I am having trouble finding a supplier with the capability of making large diameter (~55 ") flash welded rings in high temperature alloys such as RA 330 and Inconel 601. Does anyone have any suggestions?
 
The main issue is not whether there are capable facilities but more if they are willing to do only one part.
 