Can someone point me in the direction to determine the weld size, and effective throat to weld a tube to a plate for this to develop a moment. Tube is roughly 2" dia HSS and plate is likely 3/8". The condition is for a guardrail. Thanks

image_dorrbp.png


Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?
-Dik
 
dik,

See JAE's comment on this thread. The situation is similar, though not identical. Link
 
Here is a document for your use. Pay attention to page 33 and after. Link
 
So it's a matter of speccing a throat thickness... something like 1/4" or something like that... the weld strength is then treated like a normal fillet weld with that throat size?

Rather than think climate change and the corona virus as science, think of it as the wrath of God. Feel any better?
-Dik
 
Yes. Just make sure how to measure and specify the throat dimension, then it is treated as fillet weld.
 