thread338-270504
Hello ,
for horizontal flare (flare piping - buried to burn pit):
during flare scenario, MDMT is -95 deg C and service is sour with 5110 ppm of chlorides and 3.5 % H2S. pressure is 35psia. Client prefers to select alloy 625 pipe material. Now question is about last spool (around 12 m) including so-called flare tip (which in fact is pipe open end itself), process team calculated 1650 deg C and material has to be selected for this high temperature spool. i believe this last spool will have very less pressure like atm to 5 psia. i need your advice regarding possible materials which could withstand this temp. service is occasional only during startup. i think SSC and SCC is not a concern at such a lower pressure. i have seen SS310 flare tips and pipes up to some lengths in vertical flares but i dont have experience with such a situation and high temperature pipe. kindly share your experiences with similar situations. thanks in advance. are below options practical? design life is 20 yrs.
1. SS310
2. Inconel 625
3. Inconel 600
Hello ,
for horizontal flare (flare piping - buried to burn pit):
during flare scenario, MDMT is -95 deg C and service is sour with 5110 ppm of chlorides and 3.5 % H2S. pressure is 35psia. Client prefers to select alloy 625 pipe material. Now question is about last spool (around 12 m) including so-called flare tip (which in fact is pipe open end itself), process team calculated 1650 deg C and material has to be selected for this high temperature spool. i believe this last spool will have very less pressure like atm to 5 psia. i need your advice regarding possible materials which could withstand this temp. service is occasional only during startup. i think SSC and SCC is not a concern at such a lower pressure. i have seen SS310 flare tips and pipes up to some lengths in vertical flares but i dont have experience with such a situation and high temperature pipe. kindly share your experiences with similar situations. thanks in advance. are below options practical? design life is 20 yrs.
1. SS310
2. Inconel 625
3. Inconel 600