Hello everybody,

I would like to know what is ASTM A105 and what does RJ and RF facing mean for a flange?
Also what does the RJ and RF letters mean?
For example, I found out that the type WN means Weld Neck...

Sorry for my bad English and mistakes...
Méli :eek:)
 
Replies continue below

Recommended for you

ASTM A 105 is a common specification for carbon (0.35% max) steel forgings and piping applications including pressure containing parts, flanges, valves, etc. See the ASTM web site for a list of their standards. You may also find many ASTM specifications as incorporated by ASME with the same number preceded by S such as SA 105. Also refer to ASME B16.5 for flanges through nominal pipe size 24.
 