I'm in doubt about the flange rating/facing for reciprocating compressor. After search the previous thread there is relevant thread.
900# FF flanges ?
thread378-70856
In my case, the 1st stage has pressure less than 70 barg. Therefore, the cylinder material will be cast iron as API 618. The preliminary data sheet shows flange Class 600 FF.
I check the cast iron flange rating in ANSI B16.1. There is no Class 600 FF. Should I specify Class 800 RF? If we consider about the connection to steel flange 600 RF or RTJ. Should we revise the data sheet?
Please comment.
900# FF flanges ?
thread378-70856
In my case, the 1st stage has pressure less than 70 barg. Therefore, the cylinder material will be cast iron as API 618. The preliminary data sheet shows flange Class 600 FF.
I check the cast iron flange rating in ANSI B16.1. There is no Class 600 FF. Should I specify Class 800 RF? If we consider about the connection to steel flange 600 RF or RTJ. Should we revise the data sheet?
Please comment.