My colleague is trying to do a 10" blind and flange repair at the end of a header in a Sec 1 boiler. They don't have access to the outside of the flange and were wondering if they can machine the pipe/flange so that a full pen butt weld is done from the inside of the pipe. I couldn't think of a reason why not. Does anyone see an issue with that?
 
Yes. Tell him to take a 10 inch pipe to the workshop, clamp it in place - JUST AS IT WILL BE DONE IN THE FIELD, put a 10 inch flange on the end and try to prep it, fit it, and weld it from the inside.
 
No problem at all.
As long as you can produce a full penetration weld (if that is what is required) then you are good to go. How you produced the FP weld does not matter.
However, racookpe1978 has made a valid point - if you can't achieve a sound joint via mock-up in the workshop you have no hope in the field / boiler.
Cheers,
DD
 
Thanks for the responses!
 
There exists ID bore orbital welders that can provide a full pen weld from the ID. Incidentally , the max stress during startup of the boiler will be at the ID of this weld if the flange is not supplied as a "weld neck" flange; the temperature difference between the flange face and the pipe ID is significant during statup, and if the ID has a root pass defect ( as would occur if welded from the OD) then a crack can be formed from thermal stress at that defect. So, welding from the ID has the advantage of avoiding the root pass defect at the ID.

"Nobody expects the Spanish Inquisition!"
 