Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Flange Groove Inlay

Status
Not open for further replies.

Mechh007

Mechanical
Jun 21, 2012
41
Hi,
As per our client spec there is no detail about groove inlays for API 6BX flanges and we placed the material orders without inlays. Is it ok? The flange material is AISI 4130 and gasket material is SS16.


Thanks,
BN
 
Replies continue below

Recommended for you

It depends on what material class of the body want to become.
If the body was expected to have material class HH, then you have to apply cladding on the groove.

 