Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Flame Cutting to remove temporary attachments

Status
Not open for further replies.

napster385

Petroleum
Joined
Apr 4, 2013
Messages
34
Location
PH
Hi Everyone,

Is there a provision in the ASME VIII code that prohibits flame cutting as a procedure to remove welding connecting the temporary attachments such as lifting lugs to the shell or head plate of a pressure vessel?

Appreciate any response.

Thanks.
 
Nothing that prohibits this in Section VIII, Div. 1.

The section below could be used as a reference.

UG-76 CUTTING PLATES AND OTHER STOCK
(a) Plates, edges of heads, and other parts may be cut to shape and size by mechanical means such as machining,
shearing, grinding, or by oxygen or arc cutting. After oxygen or arc cutting, all slag and detrimental discoloration of
material which has been molten shall be removed by mechanical means prior to further fabrication or use.
 