Anybody knows labs that perform fire safe tests API607, please?
 
Southwest Research in San Antonio
Yarmonth Boston
 
Firmino,
where are you based?

Maybe you'll find useful to take a look at Thread408-114236 within this Forum (where European lab's are also listed...).

Hope this helps, 'NGL
 
Yarmouth Research is in Yarmouth, Maine
 
Firmino,

My experience is SwRI is best choice. One test according to API607 will cost about $3000,- Score is 3 times more expensive. The only thing i had to add was the transport costs, but still cheaper. SwRI is a certified institute and ABS will except the report without witnessing the actual test.
 
Firmino,
which edition of API 607 standard are you applying?

Please refer to thread182-133010...

Thanks, 'NGL
 