We are trying to determine how much U metel, machine cuttings, to use in a test to see if a new extinguishing agent is viable.

1. How much should the U metal machine cuttings weigh?
2. If we test it on a solid piece of U metal what should the size and weight of the U metal be?
3. How many times should we repeat the test?
4. If we use a solid piece in #2 above how do we ignite it?

Thanks for the assistance in advance.
 