Hi guys!
I being in a pharma company, we fancy covering everything in stainless steel sheets. To reduce time scales, nowadays, prebuffed SS304 sheets are used. When you peel off the sticker on the sheets, the become prone to finger prints even if you have clean hands (washed by IPA, and don't suspect IPA
). First I tried soap solution but it leaves dark patches and they are very much visible at the illumination level of above 500 lux (and this is the minimum level). I tried HNO3 and K2Paste (I don't know what you call it at your place) but not to my help.
I will be a happy soul if I get some sort of solution.
Thanks in advance,
Believe it or not : If a person becomes invisible, he/she becomes blind as well.
I being in a pharma company, we fancy covering everything in stainless steel sheets. To reduce time scales, nowadays, prebuffed SS304 sheets are used. When you peel off the sticker on the sheets, the become prone to finger prints even if you have clean hands (washed by IPA, and don't suspect IPA
![[wink] [wink] [wink]](/data/assets/smilies/wink.gif)
I will be a happy soul if I get some sort of solution.
Thanks in advance,
Believe it or not : If a person becomes invisible, he/she becomes blind as well.