Nov 26, 2003 #1 begs Mechanical Joined Jul 30, 2003 Messages 1 Location US I'm having a lot of trouble finding the steel property info I need for a design. I have a fatigue condition and need S-N diagrams or at least an endurance limit for 300M and 350 Maraging steels. Can anyone point me to a good spot on-line?
I'm having a lot of trouble finding the steel property info I need for a design. I have a fatigue condition and need S-N diagrams or at least an endurance limit for 300M and 350 Maraging steels. Can anyone point me to a good spot on-line?
Nov 26, 2003 #2 mirekp Mechanical Joined Sep 7, 2002 Messages 49 Location CZ Try next links: http://www.key-to-steel.com/default.htmhttp://www.matweb.com Mirekp http://www.mitcalc.comMechanical calculations Upvote 0 Downvote
Try next links: http://www.key-to-steel.com/default.htmhttp://www.matweb.com Mirekp http://www.mitcalc.comMechanical calculations
Nov 26, 2003 #3 israelkk Aerospace Joined Dec 30, 2002 Messages 2,280 Location IL 300M S/N curves and more data appears in MIL-HDBK-5J availabe from http://assist.daps.dla.mil/quicksearch/ Upvote 0 Downvote
300M S/N curves and more data appears in MIL-HDBK-5J availabe from http://assist.daps.dla.mil/quicksearch/