Hey
Can anyone recommend me a filter for filtering fly ashes from a liquid stream of a continuous process. The flow rate is 2-3 l/min.
Thanks
Extassi
 
You need to check this site for duplex or twin strainer setup.
This will get you by for a lot less money if the ash loading isn’t too high. Download the pdf brochure on strainers.


If the loading on the liquid stream is very high you may have to go to a continious screener.
Come back with some information on loadings (ash).
 
What flyash, (combustion product), what liquid, what pressure, what temperature, what level of purity desired, what, what, what. Help us help you. Thanks for at least telling us 2-3l/min.

rmw

 
Hi
Yes its a combustion product. The liquid flow rate is 2-3 l/min, ash content is about 4 g/l. Max. temp. is 50 °C and pH is between 6-7.
regards