Does anyone have a suggestion on a perferred FCAW all postion welding wire. We are currently using tri-mark(e71t-1) and ending up with prosity and worm tracks in our weld. Our sheilding gas is good; no fans are in the work areas. Any suggestions on what could be causing these defects?
Also many of our welders are failing VT inspections due to slag inclustions. Any tips on what to tell these welders to prevent this kind of mistakes.I am a welder by trade but now in QA/QC; I never had this problem over and over. My conclustion is the welder is running to cold and not staying in there weld puddle.
Any suggestions will help.
thank you all,
Also many of our welders are failing VT inspections due to slag inclustions. Any tips on what to tell these welders to prevent this kind of mistakes.I am a welder by trade but now in QA/QC; I never had this problem over and over. My conclustion is the welder is running to cold and not staying in there weld puddle.
Any suggestions will help.