stillfan

Structural
Jan 18, 2010
35
I have been reading alot about welding for cold formed memebers (11 and 13 gauge)have found that they recommend GMAW,SMAW and FCAW. I also read in AISC 13th edition that fillet welds do not prequalify for GMAW. I have some shop dwgs with fillet welds shown all over the cold formed connections.

Does AWS D1.3 have an allowance for GMAW fillet welds?

If not then I assume that SMAW or FCAW would be prequalified, is this correct?
 
Replies continue below

Recommended for you

yes GMAW fillets are prequalified (with limites), review AWS 1.3 2008 para 3.2.2 and figure 3.2A, 3.2B, and 3.2C.
 
Thank you, I do not have access to AWS 1.3 would you highlight the limits or post these sections.

Thanks again
 