Can smene tell me if I should put tha NA at the center or somewhat lower say 1/3 up frm the bottom surface when calculating S from stress = M/S. It seams the compression side has more area than the tensin side due to the base material thickness plus the fillet weld area. I just think it should be lower than the 1/2 point. For example, lets say I have a 2x2 square tube with wall thickness of 1/4". I put a 1/4" fillet weld all around. The load is 500 lbs at a distance of 10".
Also, do I use the throat area to calculate S? And do I consider this load to be shear acting on throat area so use .3UTS of weld material to determine safety factor. And what SF is typical? I'm thinking of 2.5 to 1. Is this reasonable?
Thanks
Also, do I use the throat area to calculate S? And do I consider this load to be shear acting on throat area so use .3UTS of weld material to determine safety factor. And what SF is typical? I'm thinking of 2.5 to 1. Is this reasonable?
Thanks