I have been working on standardizing headers for boilers . one of the most important issue is the fillet weld size for tubes of 4mm thick.
->an example is for a 200 NB pipe of lets say SCH 120 I am going to have tubes of 63.5 mm OD at a spacing of 101.9. I have calculated the pipe thickness based on ligament efficiency. The tubes are kind of set on on the header pipe with a some depth for groove 6mm and the fillet weld size as per some old standard is 9mm(6mm throat size).
The Questions are:
1) is it practical to have a 9mm fillet weld with a groove of 6 mm deep for a tube thickness of 4mm.
2) do we need to do weld strenght calculation as we do for tubes in tubesheet of heat exchanger (full strengtt welded,partial strenght welded), which I think if I am not wrong refers to the stenght based on tube, full strength weld mean that if tube is pull the tube will fail but the joint won,t get failed? am I right as per this understanding?
3) considering the pipe thickness is based on ligament efficiency , do we need to do the weld strenght calcualtions as mentioned in ASME SEC VIII DIV 1 or ASME I where weld strength required is based on area required fo rreinforcement.
Please suggest ..too much confusion on my side..
Thanks
->an example is for a 200 NB pipe of lets say SCH 120 I am going to have tubes of 63.5 mm OD at a spacing of 101.9. I have calculated the pipe thickness based on ligament efficiency. The tubes are kind of set on on the header pipe with a some depth for groove 6mm and the fillet weld size as per some old standard is 9mm(6mm throat size).
The Questions are:
1) is it practical to have a 9mm fillet weld with a groove of 6 mm deep for a tube thickness of 4mm.
2) do we need to do weld strenght calculation as we do for tubes in tubesheet of heat exchanger (full strengtt welded,partial strenght welded), which I think if I am not wrong refers to the stenght based on tube, full strength weld mean that if tube is pull the tube will fail but the joint won,t get failed? am I right as per this understanding?
3) considering the pipe thickness is based on ligament efficiency , do we need to do the weld strenght calcualtions as mentioned in ASME SEC VIII DIV 1 or ASME I where weld strength required is based on area required fo rreinforcement.
Please suggest ..too much confusion on my side..