In qualifying a PQR to ASME Sec IX, QW 181, where testing will be to QW 183, with no mechanical tests involved, is PWHT an essential variable?
 
Replies continue below

Recommended for you

Weldtek;
If you intend to qualify a fillet weld WPS in a situation where PWHT is required by Code for fillet welds, yes, PWHT should be included as an essential welding variable for this procedure.
 