connectegr
Structural
What is the "correct" detail for the attached skewed T Joint? The specifics are for plate thicknesses 3/8" or less, with an angle of 30* or less. A detailed root opening of 3/16" or less.
I have typically seen and provided the detail as shown in Option A. The other-side fillet weld is increased to account for the detailed root opening. Thus the fillet weld detail is shown with unequal sizes. This is also shown in the AISC 13th Edition, Table 10-13.
However, I am presently reviewing design calculations and details provide using Design Data's SDS2. The details are shown as Option B. The calculations refer to AWS D1.1 Figure 3.11. And the shop drawings show welds of equal size.
My concern is that with Option B the welder does not know that the weld size shown are effective leg sizes. And that much more than a single pass weld is required.
I have typically seen and provided the detail as shown in Option A. The other-side fillet weld is increased to account for the detailed root opening. Thus the fillet weld detail is shown with unequal sizes. This is also shown in the AISC 13th Edition, Table 10-13.
However, I am presently reviewing design calculations and details provide using Design Data's SDS2. The details are shown as Option B. The calculations refer to AWS D1.1 Figure 3.11. And the shop drawings show welds of equal size.
My concern is that with Option B the welder does not know that the weld size shown are effective leg sizes. And that much more than a single pass weld is required.