Sep 24, 2009 #1 engineermat Mechanical Joined Mar 17, 2008 Messages 47 Location US What filler metal should be used for 316/316L Stainless Steel to Alloy 20 welding (GTAW process) Thanks a lot.
What filler metal should be used for 316/316L Stainless Steel to Alloy 20 welding (GTAW process) Thanks a lot.
Sep 24, 2009 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US I would use an Inconel filler metal 625. Upvote 0 Downvote
Sep 25, 2009 #3 EdStainless Materials Joined May 20, 2004 Messages 16,373 Location Waukesha WI USA I thought that I had a better idea, but practically speaking 625 will be the easiest to find. However, since the weld needs no better corrosion resistance than 316 you could get away with simply using Alloy 20 weld filler. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
I thought that I had a better idea, but practically speaking 625 will be the easiest to find. However, since the weld needs no better corrosion resistance than 316 you could get away with simply using Alloy 20 weld filler. = = = = = = = = = = = = = = = = = = = = Plymouth Tube
Sep 25, 2009 #4 mock1 Industrial Joined Sep 23, 2009 Messages 10 Location US I'm not understanding why this needs to be done. Why not use 321SS if this is for acid the 316 won't hold out as long without pitting. Upvote 0 Downvote
I'm not understanding why this needs to be done. Why not use 321SS if this is for acid the 316 won't hold out as long without pitting.