What filler metal should be used for 316/316L Stainless Steel to Alloy 20 welding (GTAW process)

Thanks a lot.
 
Replies continue below

Recommended for you

I thought that I had a better idea, but practically speaking 625 will be the easiest to find.

However, since the weld needs no better corrosion resistance than 316 you could get away with simply using Alloy 20 weld filler.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
I'm not understanding why this needs to be done. Why not use 321SS if this is for acid the 316 won't hold out as long without pitting.
 