H.P. Steam 90bar 490C (1300psi 914F)
When we have to repair pipework during shutdown if we cannot Hyd. Press. test the pipework we 100% Radiograph all Final butt welds (butt welds are the only weld we allow as final welds even down to sizes we would normally use Socket weld fittings on).
While I agree with this on pipework that is going to be stressed
Is it acceptable to use a Socket weld fitting on small short lines (vents & drains with no stress)without having done anything other than MPI ?
I just need some advice on this as I cannot find any literature to back up my gut feeling.
When we have to repair pipework during shutdown if we cannot Hyd. Press. test the pipework we 100% Radiograph all Final butt welds (butt welds are the only weld we allow as final welds even down to sizes we would normally use Socket weld fittings on).
While I agree with this on pipework that is going to be stressed
Is it acceptable to use a Socket weld fitting on small short lines (vents & drains with no stress)without having done anything other than MPI ?