Hi all,
I understand that 2 part epoxy is common for FBE open cut pipe materials, for bore section where it has to be pulled and coated with ARO for abrasion, what are some options for a good coating for that situation. I'm thinking something in the power crete line but have not experience in that..
thanks for your help.
As much as possible, do it right the first time...
I understand that 2 part epoxy is common for FBE open cut pipe materials, for bore section where it has to be pulled and coated with ARO for abrasion, what are some options for a good coating for that situation. I'm thinking something in the power crete line but have not experience in that..
thanks for your help.
As much as possible, do it right the first time...