Does somebody have problems cutting ss201LN. Me not stable at all. And have to film burning before. I tried low speed like 75in/minute as like 235in/minute. I tried gas from 15 bar to 20 bar. I tried focal like -3.9 to -5.6 and Stil Nevers good. That for 1/4. Got à bit less problems with 7 ga.
 